How do you airless spray epoxy and PU coatings on steel?

Prepare the steel to the specified standard, mix the two-pack epoxy and let it induct if required, spray within pot life using the tip and pressure from the data sheet, check wet and dry film thickness, then apply the polyurethane topcoat within the recoat window. Flush the equipment before the coating cures.

Epoxy primers and polyurethane topcoats are the backbone of protective coating systems on steel in Delhi NCR plants, warehouses and fabrication yards. They are also the coatings that punish careless application. Two-pack products have a limited pot life, strict recoat windows and specified film thickness. Airless spraying is the standard way to apply them on large steel, but only if the whole process is controlled. This guide walks through the practical steps. It is general guidance. The Jotun data sheet for your product and the Graco manual for your machine always come first.

Why epoxy and PU are used together

A typical protective system on exposed steel has three roles:

  • Epoxy primer bonds to the prepared steel and gives the first barrier against moisture and corrosion.
  • Epoxy build coat adds film thickness, which lengthens the path moisture must take to reach the steel.
  • Polyurethane topcoat protects the epoxy from sunlight, which would otherwise chalk and fade it, and keeps colour and gloss.

Jotun families commonly used for these layers include Penguard for epoxy primers and build coats and Hardtop for polyurethane topcoats. The exact product, number of coats and thickness depend on the exposure and specification, so see our protective coatings page and ask us to match a system to your asset.

Step 1: Surface preparation decides the result

No sprayer can rescue a badly prepared surface. Most early coating failures trace back to preparation.

  • Degrease first. Remove oil, grease and process residues before any blasting or grinding.
  • Remove rust, scale and old paint to the standard in the data sheet or specification. Abrasive blasting to a specified cleanliness grade is common for demanding exposure; some jobs use power tool cleaning where blasting is not possible.
  • Achieve the surface profile the primer requires. The profile gives the coating something to grip.
  • Remove dust. Blast dust left on the surface prevents bonding. Vacuum or blow clean with dry, oil-free air.
  • Prime quickly. Blasted steel can flash rust in hours in monsoon humidity, so schedule priming soon after blasting.
  • Stripe coat welds, edges and bolts by brush before the main coat, since these areas are the first to fail.

Step 2: Check the weather and the steel

Two-pack coatings are sensitive to conditions at the time of application. The data sheet states limits for steel temperature, air temperature and humidity.

  • Steel temperature should stay a safe margin above the dew point. Damp steel traps moisture under the film.
  • In 45 degrees C summers, steel in the sun can be much hotter than the air. Hot steel causes dry spray, solvent popping and poor flow. Work early in the day or in the shade.
  • In monsoon months, humidity delays curing and risks condensation overnight. Plan around dry spells and covered areas.
  • In winter, low temperatures slow curing, and some epoxies may not cure properly if too cold. Check the minimum temperature in the data sheet.
  • Smog and dust settle on wet coatings. Avoid windy, dusty hours.

Step 3: Mixing, induction and pot life

Epoxy and polyurethane coatings are usually supplied in two components, a base and a hardener. Once mixed, a chemical reaction begins that cannot be stopped.

  1. Use the correct ratio. Mix full kits wherever possible. Splitting kits invites ratio errors.
  2. Stir the base first with a power mixer until uniform, then add the hardener and mix again.
  3. Respect induction time if the data sheet requires it. Some products need a waiting period after mixing before they are ready to spray.
  4. Know your pot life. This is the time after mixing during which the product can be applied. It shortens as temperature rises. In summer heat it can be much shorter than in winter.
  5. Mix only what you can spray within pot life. Never use mixed material that has begun to thicken or gel.
  6. Do not mix leftover material with fresh batches.

Step 4: Thinning per the data sheet

Thinning changes the coating. Add thinner only when the data sheet allows it, only the type it names and never above the stated limit. Over-thinning lowers the solids content, so the film comes out thinner than expected and its protection is reduced. If a coating sprays poorly, check temperature, mixing and tip before reaching for the thinner can. Add thinner after mixing the components, not before.

Step 5: Set up the airless equipment

Epoxies and PU are typically sprayed with a suitable airless sprayer. Graco offers a range, and your choice depends on the area, the coating and the number of guns. The Ultra Max II 490 reaches up to 2.0 L/min and 228 bar, the Ultra Max II 695 reaches up to 2.8 L/min at 227 bar, and the GMAX II 3900 reaches up to 4.73 L/min at 228 bar with up to two guns. Larger structures may benefit from the GMAX II 5900 or 7900. See the full range on our Graco airless sprayers page.

  • Choose the tip and pressure from the data sheet recommendation, then confirm on a test panel.
  • Use a filter mesh suited to the coating, and strain the mixed material.
  • Check that hoses, seals and fittings are compatible with the solvents in the coating.
  • Earth the equipment and the work, and keep ignition sources away from solvent-based coatings.
  • Prime the pump and hose with the coating or the cleaning solvent recommended by the manual.

Step 6: Spray technique and film thickness

Technique controls thickness. The data sheet gives a recommended dry film thickness (DFT) per coat and a matching wet film thickness (WFT). The WFT is what you can measure while the coating is still wet, using a simple wet film gauge. It lets you correct the pass as you go, long before the coating cures.

Stage What to do What to check
Stripe coat Brush on welds, edges, bolts Full coverage, no skips
Primer Spray in even, overlapping passes WFT against data sheet
Build coat Spray after primer reaches recoat state Recoat window, DFT
Topcoat Spray PU within overcoating limits Gloss, colour, DFT
  • Hold the gun square to the surface and at a steady distance. Arcing the wrist lays thin film at the edges of each stroke.
  • Overlap each pass by about half the fan width, or as your supervisor trains.
  • Start the gun moving before you pull the trigger and release the trigger before you stop.
  • Apply cross coats on difficult areas as per the application method specified.
  • Measure DFT after curing with a dry film gauge and record readings for the client.

Step 7: Recoat windows

Every epoxy has a minimum and maximum recoat interval, and those intervals change with temperature. Recoating too soon can trap solvent. Recoating too late can leave a surface that is too smooth and hard for the next coat to grip, which may need roughening or other treatment as the data sheet states. Keep a record of the time and temperature at which each coat was applied. In hot weather, the window moves faster than most crews expect.

Step 8: Flushing and cleaning

Two-pack coatings cure inside your equipment if you let them. Flushing is not optional.

  • Flush the pump, hose and gun with the recommended cleaning solvent as soon as spraying stops, and always before pot life ends.
  • Never leave mixed material in the machine during a lunch break unless pot life clearly allows.
  • Clean the tip and filters by hand. Replace worn seals and tips.
  • Dispose of waste solvent and coating residues according to rules and site policy.
  • For storage, follow the manual’s guidance for protecting the pump.

Recording the job for the client

Consultants and plant owners increasingly ask for proof that the specification was followed. A simple site log helps you and protects your contract. For every coat, note the date, time, steel temperature, air temperature, humidity, batch numbers, mixing time, WFT readings and later DFT readings. Add photographs of the surface after preparation and after each coat. If a dispute comes up months later, this record shows that the work was done properly. It also helps your own team learn which hours and conditions give the best results at your site.

Common mistakes on epoxy and PU jobs

  • Spraying over damp or dusty steel.
  • Exceeding pot life because a batch was too large.
  • Over-thinning to make spraying easier.
  • Missing the recoat window and not recording times.
  • Skipping stripe coats on welds and edges.
  • Not measuring WFT and DFT.
  • Letting the pump sit with mixed material inside.

What to tell us when you call

  • The asset: steel structure, shed, tank, machinery or pipework, and its location.
  • Area in square metres and the number of coats in your specification.
  • The coating products, or the exposure so that we can suggest a Jotun system.
  • Surface condition and how it will be prepared.
  • Number of guns and operators, and the power supply on site.
  • Target dates, especially if a plant shutdown is involved.

Prices are not listed online. We quote on the call after we know your area and quantity, and we confirm availability then.

Talk to VTech Solution

VTech Solution is an authorised Jotun distributor and dealer and an authorised Graco distributor in Sahibabad Industrial Area, Ghaziabad, supplying contractors, factories and fabricators across Delhi NCR since 2011. Call +91 98111 70042 Monday to Saturday, 10am to 6pm, or email sales@vtechsolution.co.in. Visit our protective coatings and Graco airless sprayers pages to see the range.

Frequently asked questions

What is pot life and why does it matter for epoxy and PU?

Pot life is the time after mixing the base and hardener during which the coating can still be applied. It shortens in Delhi NCR summer heat. Material past its pot life thickens and fails to apply properly. Check the Jotun data sheet and mix only what you can spray.

Can I thin epoxy or PU for airless spraying?

Only as the data sheet allows, using the thinner type and maximum amount it names. Over-thinning lowers solids and gives a thinner film than intended. If spraying is difficult, first check temperature, mixing, tip size and filters.

What is the difference between WFT and DFT?

Wet film thickness (WFT) is measured while the coating is wet, using a wet film gauge, so you can correct as you spray. Dry film thickness (DFT) is measured after curing with a dry film gauge. The data sheet gives both targets for each coat.

Why must I flush the sprayer after two-pack coatings?

Epoxy and polyurethane cure by chemical reaction, so mixed material hardens inside the pump, hose and gun if left. Flush with the recommended cleaning solvent before pot life ends and clean the tip and filters. Follow the Graco manual.

Which Jotun coatings are used for epoxy and PU systems?

Jotun families commonly used include Penguard for epoxy primers and build coats and Hardtop for polyurethane topcoats. The right system depends on exposure and specification. Call VTech Solution on +91 98111 70042, and we will suggest a system and quote on the call.